I spent hours doing it and on most of the walls the cracks were no longer there and on others they were very very faint but I couldn't get them any better. Happy with that I rubbed the walls down to ensure there was as little dust as possible clinging to them.
I put another coat of paint on, manually and careful to be conservative with the amount of paint on the roller. Sadly all the walls cracked again after just the first coat. I was at my wits end at the countless hours spent and the amount of dust created and I had made no headway. I did find a solution and that was to use something that perhaps I should have used right from the get go.
I didn't even sand the walls down, I put the Polycell 3 In 1 Basecoat over the cracked paint and it smoothed it out instantly, one 5L tub did the whole of the decent sized bedroom.
I gave it 24 hours to dry and put the first coat of paint on, which I had thinned out before the previous failed attempt after the sanding. The first coat looked very patchy but it didn't crack. A couple of days later I put the second coat on, a proper not thinned coat and it went on beautifully, didn't crack and didn't require any more coats. I'm finally happy with the room and wouldn't hesitate to recommend the same solution for any room with a dominant colour that needs replacing.
It's not a cheap solution but neither is it expensive and it makes up for it in the labour time saved. I have another room to do soon, I'll not be doing it for a couple of weeks but I'm very tempted to use the Polycell 3 In 1 Basecoat to cover the green before I go at it with the proper colour. I hope you get similar success with whatever method you choose to remedy your issue.
PGibsonCoUk , 14 Feb Morning all. You haven't said what type of paint was originally on the walls or what type of paint you are using. You can certainly get this sort of cracking if you use matt emulsion over silk emulsion. HumpyD , 15 Feb Matt does crack over silk but it cant be that as he says he stripped the ceiling. Its because you used PVA to seal it. Anything you put on top of the PVA will adhere poorly, so its risky.
You'd be better off trying to remove as much of the PVA as possible by dry scraping and washing. Thanks for your reply.
I will definitely give that a go with the polycell underneath, anything is better than sanding down all the walls! I also put some smooth it on the ceiling where the light fitting has been moved and then i sanded and painted over that, and that is cracking aswell! Gomezbess26 I realise this is an old thread but did the polycell work? I have the same issue I sanded back to the silk layer gave it a key put some dulux soft sheen instead on matt paint on but it has cracked. Really don't want to have to sand the walls down again.
Many thanks. Jimbob88 , 26 Aug I had a similar issue and used a solvent based undercoat prior to overcoat in with Matt emulsion. Worked a treat. Can you remember what brand solvent undercoat was? Show more Show less. Successfully registered, please login Login.
Password changed successfully. Back to my account. Back to login. We will use this to provide you with useful information. In the next month. From months. After 6 months. Living room. Dining room. Childrens room. I am decorating in order to refresh my room style e. I am decorating in order to change my room style e. Blistering and flaking Cause This may be due to any of the following factors: Moisture trapped beneath the surface of the paint film.
If the paint is applied over a powdery or friable surface. Surface contamination such as dirt, oil, and grease. Polish residues on the surface, which impair the adhesion of the paint.
Excessive movement of the substrate, such as joints, imposing stress on the paint film which can result in cracking which in turn lets in moisture, ultimately resulting in a flaking paint film. Resins present in knots causing light coloured paints to discolour or even flake.
Resin bleed and flaking is a common problem where dark colours are used on south facing elevations. This is because dark colours absorb more heat than light colours. Putting it right All loose material will have to be removed back to a firm edge, spot primed with the appropriate Dulux Primer, and then recoated with the appropriate product.
Putting it right It is important to seal the original stain by applying a coat of Polycell Stain Stop prior to re-decorating. Cissing Cause This is caused by painting over contaminated surfaces such as wax, oil or polish. Putting it right Allow the surface to dry and then rub down using 'wet and dry' abrasive paper and a solution of warm water and detergent. Filler shows through the paint Cause Filler shows through the paint. Putting it right Make sure that all filled areas are rubbed down smooth and level.
Foaming Cause Using the wrong type of roller can cause foaming of a paint film. Putting it right You will need to rub down using 'wet and dry' abrasive paper using water with a little detergent added.
Mud cracking Cause The most likely cause of mud cracking is applying a thick, heavy, unthinned coat of paint to a textured or embossed surface such as blown vinyl wallpapers or pebbledash. Putting it right One or two thinned coats of paints may fill in the cracks. Powdery or chalky surfaces on outside paint work Cause This is caused usually by a wearing away of the paint film by weathering or could be evidence of salts coming out of the surface.
Putting it right The affected area should be brushed down with a stiff bristle brush to remove as much powdery material as possible before applying a coat of Weathershield Exterior Stabilising Primer. Cracking of plaster Cause This is a common occurrence in new houses and is often the result of plaster drying out or movement of the building.
Putting it right Cracks should be cut out and all dust and debris removed. Mould growth on exterior surfaces Cause Moisture is an essential element for the growth of moulds Putting it right Affected areas should be treated with Weathershield Multi-Surface Fungicidal Wash. Putting it right Allow the paint to dry and harden. Over-thinning your paint or applying it too thinly can also cause it to split.
I used this to paint a new narrow pine bathroom door, I found it really easy to use, I like that it is quick drying, I had no problems with it at all. I think the finish is good. This is what makes paint a liquid that can be applied to a surface.
Too little water, and the paint would be thicker and less pliable. Vertical and horizontal cracks in drywall or plaster walls typically indicate drying and shrinkage, which is normal after construction. Jagged cracks, stair-step cracks and degree angle cracks generally signify structural movement or settling issues that are occasionally serious but usually harmless. A smooth and flexible paint, that permanently covers cracks and stains.
Cracking occurs in acrylic paint pours when the top layer of paint dries faster than the underlying layer. As the bottom layer dries, it pulls at the semi-hardened skin on top and when the force is too much, a crack is created.
Newly formed cracks will continue to widen until the paint is fully dried. The most likely cause of mud cracking is applying a thick, heavy, unthinned coat of paint to a textured or embossed surface such as blown vinyl wallpapers or pebbledash.
Cracking can also occur when Matt paint is applied over Silk if the sheen is not removed from the silk coating. Waiting 24 hours is best for oil-based paint and primer. Painting Over Flaking Paint Remove as much of the loose paint as possible using a flexible scraper with a good sharp edge. Skim coat the area with a good quality filler, Toupret Interior Filler is perfect for the task.